Medidas
Property | Value |
---|---|
Dimensions | Round-Bar length: 5-230 mm - Sheet: 17x15-254x63.5 mm |
Mecánica
Chemical properties
Property | Value | Comment |
---|---|---|
Azufre | 0.025 % Show Supplier Material materials with Azufre of 0.025 % | max. |
Carbono | 0.07 % Show Supplier Material materials with Carbono of 0.07 % | max. |
Cobre | 3.0 - 5.0 % Show Supplier Material materials with Cobre of 3.0 - 5.0 % | |
Cromo | 15.0 - 17.5 % Show Supplier Material materials with Cromo of 15.0 - 17.5 % | |
Fósforo | 0.025 % Show Supplier Material materials with Fósforo of 0.025 % | max. |
Manganeso | 1.0 % Show Supplier Material materials with Manganeso of 1.0 % | max. |
Niobio | 0.15 - 0.45 % Show Supplier Material materials with Niobio of 0.15 - 0.45 % | |
Níquel | 3.0 - 5.0 % Show Supplier Material materials with Níquel of 3.0 - 5.0 % | |
Silicona | 1.0 % Show Supplier Material materials with Silicona of 1.0 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Processing history | Solution Annealed |