All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

Typical for Cast 7xx.x Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

74.0 GPa

Show Material materials with Elastic modulus of 74.0 GPa

Typical for Cast 7xx.x Series Aluminium

Hardness, Brinell

150.0 [-]

Show Material materials with Hardness, Brinell of 150.0 [-]

T61

Pink Sheets, ASTM B955

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 7xx.x Series Aluminium

Tensile strength

510.0 MPa

Show Material materials with Tensile strength of 510.0 MPa

T61

Pink Sheets, ASTM B955

Thermal

PropertyValueConditionRelated StandardsComment

Coefficient of thermal expansion

2.4e-05 - 2.5e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 - 2.5e-05 1/K

Typical for Cast 7xx.x Series Aluminium

Melting point

477.0 - 635.0 °C

Show Material materials with Melting point of 477.0 - 635.0 °C

T61

Pink Sheets, ASTM B955

Specific heat capacity

963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 963.0 J/(kg·K)

Typical for Cast 7xx.x Series Aluminium

Thermal conductivity

100.0 - 160.0 W/(m·K)

Show Material materials with Thermal conductivity of 100.0 - 160.0 W/(m·K)

Typical for Cast 7xx.x Series Aluminium

Chemical properties

PropertyValueConditionRelated Standards

Chromium

0.18 - 0.28 %

Show Material materials with Chromium of 0.18 - 0.28 %

T61

Pink Sheets, ASTM B955

Copper

1.2 - 2.0 %

Show Material materials with Copper of 1.2 - 2.0 %

T61

Pink Sheets, ASTM B955

Iron

0.50 %

Show Material materials with Iron of 0.50 %

T61

Pink Sheets, ASTM B955

Magnesium

2.1 - 2.9 %

Show Material materials with Magnesium of 2.1 - 2.9 %

T61

Pink Sheets, ASTM B955

Manganese

0.3 %

Show Material materials with Manganese of 0.3 %

T61

Pink Sheets, ASTM B955

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

T61

Pink Sheets, ASTM B955

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

T61

Pink Sheets, ASTM B955

Zinc

5.1 - 6.1 %

Show Material materials with Zinc of 5.1 - 6.1 %

T61