EN 1706 Grade AC-71000 T1

Want to keep this datasheet? Save it now in your required format

Description

Material EN AC-AlZn5Mg is produced as sand and die cast. It shows the following casting characteristics and properties: plasticity: acceptable heat crack resistance: insufficient pressure tightness: insufficient workability (after heat-treatment): excellent worability (casting condition): excellent corrosion resistance: good decorative anodic oxidation: good weldability: acceptable polishability: good strength at room temperature: acceptable strength at increased temp. (up to 200°C): insufficient ductility (impact strength): good fatigue strength amounts 60 to 90 N/mm² ( best available casting method, values for vibration durability up to 50*10 hoch 6 cycles [Woehler diagram]).

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

Typical for Cast 7xx.x Series Aluminium

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

60.0 - 90.0 MPa

Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa

T1

EN 1706

Casting

Elastic modulus

74.0 GPa

Show Material materials with Elastic modulus of 74.0 GPa

Typical for Cast 7xx.x Series Aluminium

Hardness, Brinell

60.0 [-]

Show Material materials with Hardness, Brinell of 60.0 [-]

T1

EN 1706

Casting

65.0 [-]

Show Material materials with Hardness, Brinell of 65.0 [-]

T1

EN 1706

Casting

20.0 °C

60.0 [-]

Show Material materials with Hardness, Brinell of 60.0 [-]

T1

EN 1706

20.0 °C

65.0 [-]

Show Material materials with Hardness, Brinell of 65.0 [-]

T1

EN 1706

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 7xx.x Series Aluminium

Tensile strength

190.0 MPa

Show Material materials with Tensile strength of 190.0 MPa

T1

EN 1706

Casting

210.0 MPa

Show Material materials with Tensile strength of 210.0 MPa

T1

EN 1706

Casting

20.0 °C

190.0 MPa

Show Material materials with Tensile strength of 190.0 MPa

T1

EN 1706

20.0 °C

210.0 MPa

Show Material materials with Tensile strength of 210.0 MPa

T1

EN 1706

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

20 °C

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

T1

EN 1706

Casting

100.0 °C

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

T1

EN 1706

Casting

100 °C

2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.4e-05 1/K

T1

EN 1706

Casting

Melting point

550.0 - 645.0 °C

Show Material materials with Melting point of 550.0 - 645.0 °C

Typical for Cast 7xx.x Series Aluminium

Specific heat capacity

963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 963.0 J/(kg·K)

Typical for Cast 7xx.x Series Aluminium

Thermal conductivity

20.0 °C

130.0 - 140.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 140.0 W/(m·K)

T1

EN 1706

Casting

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

19000000.0 - 21000000.0 S/m

Show Material materials with Electrical conductivity of 19000000.0 - 21000000.0 S/m

T1

EN 1706

Casting

Electrical resistivity

4.76e-08 - 5.26e-08 Ω·m

Show Material materials with Electrical resistivity of 4.76e-08 - 5.26e-08 Ω·m

T1

EN 1706

Casting

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

90.3 %

Show Material materials with Aluminium of 90.3 %

T1

EN 1706

Chromium

0.15 - 0.6 %

Show Material materials with Chromium of 0.15 - 0.6 %

T1

EN 1706

Casting

Copper

0.15 - 0.35 %

Show Material materials with Copper of 0.15 - 0.35 %

T1

EN 1706

Casting

Iron

0.8 %

Show Material materials with Iron of 0.8 %

T1

EN 1706

0.80 %

Show Material materials with Iron of 0.80 %

T1

EN 1706

Casting

Lead

0.05 %

Show Material materials with Lead of 0.05 %

T1

EN 1706

Casting

Magnesium

0.4 - 0.7 %

Show Material materials with Magnesium of 0.4 - 0.7 %

T1

EN 1706

Casting

Manganese

0.4 %

Show Material materials with Manganese of 0.4 %

T1

EN 1706

Casting

Nickel

0.05 %

Show Material materials with Nickel of 0.05 %

T1

EN 1706

Casting

Silicon

0.3 %

Show Material materials with Silicon of 0.3 %

T1

EN 1706

Casting

Tin

0.05 %

Show Material materials with Tin of 0.05 %

T1

EN 1706

Casting

Titanium

0.1 - 0.25 %

Show Material materials with Titanium of 0.1 - 0.25 %

T1

EN 1706

Casting

Zinc

4.5 - 6.0 %

Show Material materials with Zinc of 4.5 - 6.0 %

T1

EN 1706

Casting

Technological properties

Property
Anodizing

decorative: good

Corrosion properties

general: good

General machinability

after thermal treatment: excellent, as cast: excellent

Processing methods

permanent mould casting, separately cast test sample