Pink Sheets Grade 850.0 T5

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

Typical for Cast 8xx.x Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

Typical for Cast 8xx.x Series Aluminium

Hardness, Brinell

45.0 [-]

Show Material materials with Hardness, Brinell of 45.0 [-]

T5

Pink Sheets, ASTM B26, ASTM B618

Casting

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 8xx.x Series Aluminium

Tensile strength

110.0 MPa

Show Material materials with Tensile strength of 110.0 MPa

T5

Pink Sheets, ASTM B26, ASTM B618

Casting

125.0 MPa

Show Material materials with Tensile strength of 125.0 MPa

T5

Pink Sheets, ASTM B108, ASTM B955

Casting

Thermal

PropertyValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

2.3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K

Typical for Cast 8xx.x Series Aluminium

Melting point

224.0 - 649.0 °C

Show Material materials with Melting point of 224.0 - 649.0 °C

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Specific heat capacity

963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 963.0 J/(kg·K)

Typical for Cast 8xx.x Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.7 - 1.3 %

Show Material materials with Copper of 0.7 - 1.3 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Iron

0.70 %

Show Material materials with Iron of 0.70 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Magnesium

0.1 %

Show Material materials with Magnesium of 0.1 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Nickel

0.7 - 1.3 %

Show Material materials with Nickel of 0.7 - 1.3 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Silicon

0.7 %

Show Material materials with Silicon of 0.7 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Tin

5.5 - 7.0 %

Show Material materials with Tin of 5.5 - 7.0 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

T5

Pink Sheets, ASTM B108, ASTM B26, ASTM B618, ASTM B955

Casting