Pink Sheets Grade A360.0 F

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.65 - 2.7 g/cm³

Show Material materials with Density of 2.65 - 2.7 g/cm³

Typical for Cast 3xx.x Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

125.0 MPa

Show Material materials with Bending Fatigue Strength of 125.0 MPa

F

Pink Sheets, ASTM B85

Casting

Elastic modulus

73.0 - 80.0 GPa

Show Material materials with Elastic modulus of 73.0 - 80.0 GPa

Typical for Cast 3xx.x Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 3xx.x Series Aluminium

Shear modulus

2.8 GPa

Show Material materials with Shear modulus of 2.8 GPa

Typical for Cast 3xx.x Series Aluminium

Tensile strength

315.0 MPa

Show Material materials with Tensile strength of 315.0 MPa

F

Pink Sheets, ASTM B85

Casting

Thermal

PropertyValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

1.6e-05 - 2.3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.3e-05 1/K

Typical for Cast 3xx.x Series Aluminium

Melting point

557.0 - 596.0 °C

Show Material materials with Melting point of 557.0 - 596.0 °C

F

Pink Sheets, ASTM B85

Casting

Specific heat capacity

960.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 960.0 - 963.0 J/(kg·K)

Typical for Cast 3xx.x Series Aluminium

Thermal conductivity

130.0 - 180.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 180.0 W/(m·K)

Typical for Cast 3xx.x Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.6 %

Show Material materials with Copper of 0.6 %

F

Pink Sheets, ASTM B85

Casting

Iron

1.30 %

Show Material materials with Iron of 1.30 %

F

Pink Sheets, ASTM B85

Casting

Magnesium

0.4 - 0.6 %

Show Material materials with Magnesium of 0.4 - 0.6 %

F

Pink Sheets, ASTM B85

Casting

Manganese

0.35 %

Show Material materials with Manganese of 0.35 %

F

Pink Sheets, ASTM B85

Casting

Nickel

0.5 %

Show Material materials with Nickel of 0.5 %

F

Pink Sheets, ASTM B85

Casting

Silicon

9.0 - 10.0 %

Show Material materials with Silicon of 9.0 - 10.0 %

F

Pink Sheets, ASTM B85

Casting

Tin

0.15 %

Show Material materials with Tin of 0.15 %

F

Pink Sheets, ASTM B85

Casting

Zinc

0.5 %

Show Material materials with Zinc of 0.5 %

F

Pink Sheets, ASTM B85

Casting