Pink Sheets Grade B443.0 F

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.65 - 2.71 g/cm³

Show Material materials with Density of 2.65 - 2.71 g/cm³

Typical for Cast 4xx.x Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

71.0 - 75.0 GPa

Show Material materials with Elastic modulus of 71.0 - 75.0 GPa

Typical for Cast 4xx.x Series Aluminium

Hardness, Brinell

40.0 [-]

Show Material materials with Hardness, Brinell of 40.0 [-]

F

Pink Sheets, ASTM B26, ASTM B618

Casting

45.0 [-]

Show Material materials with Hardness, Brinell of 45.0 [-]

F

Pink Sheets, ASTM B108

Casting

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 4xx.x Series Aluminium

Tensile strength

115.0 MPa

Show Material materials with Tensile strength of 115.0 MPa

F

Pink Sheets, ASTM B26, ASTM B618

Casting

145.0 MPa

Show Material materials with Tensile strength of 145.0 MPa

F

Pink Sheets, ASTM B108

Casting

Thermal

PropertyValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

2e-05 - 2.2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 - 2.2e-05 1/K

Typical for Cast 4xx.x Series Aluminium

Melting point

574.0 - 632.0 °C

Show Material materials with Melting point of 574.0 - 632.0 °C

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Specific heat capacity

963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 963.0 J/(kg·K)

Typical for Cast 4xx.x Series Aluminium

Thermal conductivity

130.0 - 170.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 170.0 W/(m·K)

Typical for Cast 4xx.x Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.15 %

Show Material materials with Copper of 0.15 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Iron

0.80 %

Show Material materials with Iron of 0.80 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Magnesium

0.05 %

Show Material materials with Magnesium of 0.05 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Manganese

0.35 %

Show Material materials with Manganese of 0.35 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Silicon

4.5 - 6.0 %

Show Material materials with Silicon of 4.5 - 6.0 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Titanium

0.25 %

Show Material materials with Titanium of 0.25 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting

Zinc

0.35 %

Show Material materials with Zinc of 0.35 %

F

Pink Sheets, ASTM B108, ASTM B26, ASTM B618

Casting