Pink Sheets Grade C355.0 T61

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.65 - 2.7 g/cm³

Show Material materials with Density of 2.65 - 2.7 g/cm³

Typical for Cast 3xx.x Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

73.0 - 80.0 GPa

Show Material materials with Elastic modulus of 73.0 - 80.0 GPa

Typical for Cast 3xx.x Series Aluminium

Hardness, Brinell

85.0 [-]

Show Material materials with Hardness, Brinell of 85.0 [-]

T61

Pink Sheets, ASTM B108

Casting

85.0 - 90.0 [-]

Show Material materials with Hardness, Brinell of 85.0 - 90.0 [-]

T61

Pink Sheets, ASTM B108

Casting

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 3xx.x Series Aluminium

Shear modulus

2.8 GPa

Show Material materials with Shear modulus of 2.8 GPa

Typical for Cast 3xx.x Series Aluminium

Tensile strength

275.0 MPa

Show Material materials with Tensile strength of 275.0 MPa

T61

Pink Sheets, ASTM B108

Casting

255.0 MPa

Show Material materials with Tensile strength of 255.0 MPa

T61

Pink Sheets, ASTM B108

Casting

Thermal

PropertyValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

1.6e-05 - 2.3e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.3e-05 1/K

Typical for Cast 3xx.x Series Aluminium

Melting point

546.0 - 621.0 °C

Show Material materials with Melting point of 546.0 - 621.0 °C

T61

Pink Sheets, ASTM B108

Casting

Specific heat capacity

960.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 960.0 - 963.0 J/(kg·K)

Typical for Cast 3xx.x Series Aluminium

Thermal conductivity

130.0 - 180.0 W/(m·K)

Show Material materials with Thermal conductivity of 130.0 - 180.0 W/(m·K)

Typical for Cast 3xx.x Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

1.0 - 1.5 %

Show Material materials with Copper of 1.0 - 1.5 %

T61

Pink Sheets, ASTM B108

Casting

Iron

0.20 %

Show Material materials with Iron of 0.20 %

T61

Pink Sheets, ASTM B108

Casting

Magnesium

0.4 - 0.6 %

Show Material materials with Magnesium of 0.4 - 0.6 %

T61

Pink Sheets, ASTM B108

Casting

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

T61

Pink Sheets, ASTM B108

Casting

Silicon

4.5 - 5.5 %

Show Material materials with Silicon of 4.5 - 5.5 %

T61

Pink Sheets, ASTM B108

Casting

Titanium

0.2 %

Show Material materials with Titanium of 0.2 %

T61

Pink Sheets, ASTM B108

Casting

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

T61

Pink Sheets, ASTM B108

Casting