EN 1706 Grade AC-43100 T64

Want to keep this datasheet? Save it now in your required format

Description

Aluminium casting alloy (sand casting, permanent mould casting)

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated Standards

Density

20.0 °C

2.65 g/cm³

Show Material materials with Density of 2.65 g/cm³

T64

EN 1706

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

80.0 - 110.0 MPa

Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa

T64

EN 1706, EN 13195

Casting

Elastic modulus

73.0 - 80.0 GPa

Show Material materials with Elastic modulus of 73.0 - 80.0 GPa

Typical for Cast 3xx.x Series Aluminium

Hardness, Brinell

20.0 °C

80.0 [-]

Show Material materials with Hardness, Brinell of 80.0 [-]

T64

EN 1706

80.0 [-]

Show Material materials with Hardness, Brinell of 80.0 [-]

T64

EN 1706, EN 13195

Casting

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 3xx.x Series Aluminium

Shear modulus

2.8 GPa

Show Material materials with Shear modulus of 2.8 GPa

Typical for Cast 3xx.x Series Aluminium

Tensile strength

20.0 °C

240.0 MPa

Show Material materials with Tensile strength of 240.0 MPa

T64

EN 1706

240.0 MPa

Show Material materials with Tensile strength of 240.0 MPa

T64

EN 1706, EN 13195

Casting

Thermal

PropertyTemperatureValueConditionRelated StandardsShapeComment

Coefficient of thermal expansion

100.0 °C, 100 °C, 20 °C

2.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K

T64

EN 1706, EN 13195

Casting

Melting point

505.0 - 770.0 °C

Show Material materials with Melting point of 505.0 - 770.0 °C

Typical for Cast 3xx.x Series Aluminium

Specific heat capacity

960.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 960.0 - 963.0 J/(kg·K)

Typical for Cast 3xx.x Series Aluminium

Thermal conductivity

20.0 °C

140.0 - 170.0 W/(m·K)

Show Material materials with Thermal conductivity of 140.0 - 170.0 W/(m·K)

T64

EN 1706, EN 13195

Casting

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

18000000.0 - 25000000.0 S/m

Show Material materials with Electrical conductivity of 18000000.0 - 25000000.0 S/m

T64

EN 1706, EN 13195

Casting

Electrical resistivity

4e-08 - 5.56e-08 Ω·m

Show Material materials with Electrical resistivity of 4e-08 - 5.56e-08 Ω·m

T64

EN 1706, EN 13195

Casting

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

86.9 %

Show Material materials with Aluminium of 86.9 %

T64

EN 1706

Copper

0.1 %

Show Material materials with Copper of 0.1 %

T64

EN 1706, EN 13195

Casting

Iron

0.55 %

Show Material materials with Iron of 0.55 %

T64

EN 1706

0.55 %

Show Material materials with Iron of 0.55 %

T64

EN 1706, EN 13195

Casting

Lead

0.05 %

Show Material materials with Lead of 0.05 %

T64

EN 1706, EN 13195

Casting

Magnesium

0.2 - 0.45 %

Show Material materials with Magnesium of 0.2 - 0.45 %

T64

EN 1706, EN 13195

Casting

Manganese

0.45 %

Show Material materials with Manganese of 0.45 %

T64

EN 1706, EN 13195

Casting

Nickel

0.05 %

Show Material materials with Nickel of 0.05 %

T64

EN 1706, EN 13195

Casting

Silicon

9.0 - 11.0 %

Show Material materials with Silicon of 9.0 - 11.0 %

T64

EN 1706, EN 13195

Casting

Tin

0.05 %

Show Material materials with Tin of 0.05 %

T64

EN 1706, EN 13195

Casting

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

T64

EN 1706, EN 13195

Casting

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

T64

EN 1706, EN 13195

Casting

Technological properties

Property
Anodizing

decorative: not recommended

Corrosion properties

general: good to acceptable

General machinability

after thermal treatment: good to acceptable, as cast: good

Processing methods

permanent mould casting, separately cast test sample