EN 1706 Grade AC-44200 F

Want to keep this datasheet? Save it now in your required format

Description

Aluminium casting alloy (sand casting, permanent mould casting)

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueConditionRelated StandardsShape

Density

2.65 g/cm³

Show Material materials with Density of 2.65 g/cm³

F

EN 1706, EN 13195

Casting

20.0 °C

2.65 g/cm³

Show Material materials with Density of 2.65 g/cm³

F

EN 1706

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Bending Fatigue Strength

60.0 - 90.0 MPa

Show Material materials with Bending Fatigue Strength of 60.0 - 90.0 MPa

F

EN 1706, EN 13195

Casting

Elastic modulus

75.0 GPa

Show Material materials with Elastic modulus of 75.0 GPa

F

EN 1706, EN 13195

Casting

20.0 °C

75.0 GPa

Show Material materials with Elastic modulus of 75.0 GPa

F

EN 1706

Hardness, Brinell

50.0 [-]

Show Material materials with Hardness, Brinell of 50.0 [-]

F

EN 1706, EN 13195

Casting

55.0 [-]

Show Material materials with Hardness, Brinell of 55.0 [-]

F

EN 1706, EN 13195

Casting

20.0 °C

50.0 [-]

Show Material materials with Hardness, Brinell of 50.0 [-]

F

EN 1706

20.0 °C

55.0 [-]

Show Material materials with Hardness, Brinell of 55.0 [-]

F

EN 1706

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 4xx.x Series Aluminium

Tensile strength

150.0 MPa

Show Material materials with Tensile strength of 150.0 MPa

F

EN 1706, EN 13195

Casting

170.0 MPa

Show Material materials with Tensile strength of 170.0 MPa

F

EN 1706, EN 13195

Casting

20.0 °C

150.0 MPa

Show Material materials with Tensile strength of 150.0 MPa

F

EN 1706

20.0 °C

170.0 MPa

Show Material materials with Tensile strength of 170.0 MPa

F

EN 1706

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

20 °C

1.9999999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.9999999999999998e-05 1/K

F

EN 1706, EN 13195

Casting

20 °C

2.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K

F

EN 1706, EN 13195

Casting

20 °C

2.2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2e-05 1/K

F

EN 1706, EN 13195

Casting

100 °C

1.9999999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.9999999999999998e-05 1/K

F

EN 1706, EN 13195

Casting

100.0 °C

2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 1/K

F

EN 1706

200 °C

2.1e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K

F

EN 1706, EN 13195

Casting

300 °C

2.2e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2e-05 1/K

F

EN 1706, EN 13195

Casting

Melting point

570.0 - 580.0 °C

Show Material materials with Melting point of 570.0 - 580.0 °C

F

EN 1706, EN 13195

Casting

Specific heat capacity

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

F

EN 1706, EN 13195

Casting

20.0 °C

900.0 J/(kg·K)

Show Material materials with Specific heat capacity of 900.0 J/(kg·K)

F

EN 1706

Thermal conductivity

20.0 °C

140.0 - 170.0 W/(m·K)

Show Material materials with Thermal conductivity of 140.0 - 170.0 W/(m·K)

F

EN 1706, EN 13195

Casting

Electrical

PropertyTemperatureValueConditionRelated StandardsShape

Electrical conductivity

20.0 °C

17000000.0 - 24000000.0 S/m

Show Material materials with Electrical conductivity of 17000000.0 - 24000000.0 S/m

F

EN 1706, EN 13195

Casting

Electrical resistivity

4.17e-08 - 5.88e-08 Ω·m

Show Material materials with Electrical resistivity of 4.17e-08 - 5.88e-08 Ω·m

F

EN 1706, EN 13195

Casting

Chemical properties

PropertyValueConditionRelated StandardsShape

Aluminium

85.15 %

Show Material materials with Aluminium of 85.15 %

F

EN 1706

Copper

0.05 %

Show Material materials with Copper of 0.05 %

F

EN 1706, EN 13195

Casting

Iron

0.55 %

Show Material materials with Iron of 0.55 %

F

EN 1706, EN 13195

Casting

0.65 %

Show Material materials with Iron of 0.65 %

F

EN 1706

Manganese

0.35 %

Show Material materials with Manganese of 0.35 %

F

EN 1706, EN 13195

Casting

Silicon

10.5 - 13.5 %

Show Material materials with Silicon of 10.5 - 13.5 %

F

EN 1706, EN 13195

Casting

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

F

EN 1706, EN 13195

Casting

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

F

EN 1706, EN 13195

Casting

Technological properties

Property
Anodizing

decorative: not recommended

Corrosion properties

general: good

General machinability

after thermal treatment: acceptable

Processing methods

permanent mould casting, separately cast test sample