Description

Material EN AC-AlSi9Cu3(Fe) is produced as diecast. It shows the following casting characteristics and properties: plasticity: good heat crack resistance: good pressure tightness: acceptable workability (after heat-treatment): good corrosion resistance: insufficient decorative anodic oxidation: not advisable weldability: unsuitable polishability: acceptable strength at room temperature: good strength at increased temp. (up to 200°C): good ductility (impact strength): insufficient fatigue strength amounts 60 to 90 N/mm² ( best available casting method, values for vibration durability up to 50*10 hoch 6 cycles [Woehler diagram]). Diecasting weldability depends on the embedded gas amount and is mostly insufficient. For certain casting methods are achievable good to acceptable values. To the comparable DIN-mark GD-AlSi9Cu3, mat. No. 3.2163, acc. to DIN 1725-2 : 1986-02 applies: The material an all-round alloy of excellent casting properties and high machinability. It has a lower tendency to cavities and it is mostly unhardened. It is suitable for complex, thin-walled, pressure tight, vibration resistant and impact loaded casting parts. Application: Complex machine and engine parts for vehicle industry, e-technics, mining etc., crank and other cases, electro engine parts, end shields and brackets, cylinder heads, paneling etc.

Related Standards

Equivalent Materials

Ashby charts

See where EN 1706 Grade AC-46000 F falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.75 g/cm³ at 20 °C

Mechanical

Elastic modulus

E

75 GPa at 20 °C

Show 3xx.x materials with Elastic modulus of 75 GPa at 20 °C

Elongation A50

A50

0.5 - 1 % at 20 °C

Show 3xx.x materials with Elongation A50 of 0.5 - 1 % at 20 °C

Hardness, Brinell

HB

80 [-] at 20 °C

Show 3xx.x materials with Hardness, Brinell of 80 [-] at 20 °C

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 3xx.x materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Cast 3xx.x Series Aluminium

Shear modulus

G

2.8 GPa at 20 °C

Show 3xx.x materials with Shear modulus of 2.8 GPa at 20 °C

Typical for Cast 3xx.x Series Aluminium

Tensile strength

Rm

240 MPa at 20 °C

Show 3xx.x materials with Tensile strength of 240 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

140 MPa at 20 °C

Show 3xx.x materials with Yield strength Rp0.2 of 140 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.1E-5 1/K at 20 °C

Hide chart

Melting point

Tm

490 - 600 °C

Specific heat capacity

cp

880 J/(kg·K) at 20 °C

Thermal conductivity

λ

110 - 120 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

1.30E+7 - 1.70E+7 S/m at 20 °C

Electrical resistivity

ρel

5.88E-8 - 7.69E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.25, Rest Al

Al

79.6 %

Si

8 - 11 %

Cu

2 - 4 %

Fe

1.3 %

More

Technological properties

Anodizing

decorative: not recommended

Corrosion properties

general: not sufficient

General machinability

after thermal treatment: good

Processing methods

pressure die casting, separately cast test sample

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.