GB 1173 Grade ZL207 T5

Want to keep this datasheet? Save it now in your required format

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.75 g/cm³

Show Material materials with Density of 2.75 g/cm³

Typical for Cast 1xx.x Series Aluminium

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

Typical for Cast 1xx.x Series Aluminium

Hardness, Brinell

75.0 [-]

Show Material materials with Hardness, Brinell of 75.0 [-]

T5

GB 1173

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 1xx.x Series Aluminium

Tensile strength

165.0 MPa

Show Material materials with Tensile strength of 165.0 MPa

T5

GB 1173

175.0 MPa

Show Material materials with Tensile strength of 175.0 MPa

T5

GB 1173

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.8e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.8e-05 - 2.4e-05 1/K

Typical for Cast 1xx.x Series Aluminium

Melting point

643.0 - 657.0 °C

Show Material materials with Melting point of 643.0 - 657.0 °C

Typical for Cast 1xx.x Series Aluminium

Thermal conductivity

209.0 - 222.0 W/(m·K)

Show Material materials with Thermal conductivity of 209.0 - 222.0 W/(m·K)

Typical for Cast 1xx.x Series Aluminium

Chemical properties

PropertyValueConditionRelated Standards

Iron

0.60 %

Show Material materials with Iron of 0.60 %

T5

GB 1173

Magnesium

0.15 - 0.25 %

Show Material materials with Magnesium of 0.15 - 0.25 %

T5

GB 1173

Manganese

0.9 - 1.2 %

Show Material materials with Manganese of 0.9 - 1.2 %

T5

GB 1173

Nickel

0.2 - 0.3 %

Show Material materials with Nickel of 0.2 - 0.3 %

T5

GB 1173

Silicon

1.6 - 2.0 %

Show Material materials with Silicon of 1.6 - 2.0 %

T5

GB 1173

Zinc

0.2 %

Show Material materials with Zinc of 0.2 %

T5

GB 1173

Zirconium

0.15 - 0.25 %

Show Material materials with Zirconium of 0.15 - 0.25 %

T5

GB 1173