General
Property | Value | Condition | Related Standards |
---|---|---|---|
Density | 2.65 g/cm³ Show Material materials with Density of 2.65 g/cm³ | T6 | EN 1706 |
Mechanical
Property | Value | Condition | Related Standards | Comment |
---|---|---|---|---|
Bending Fatigue Strength | 80.0 - 110.0 MPa Show Material materials with Bending Fatigue Strength of 80.0 - 110.0 MPa | T6 | EN 1706 | |
Elastic modulus | 74.0 GPa Show Material materials with Elastic modulus of 74.0 GPa | T6 | EN 1706 | |
Hardness, Brinell | 75.0 [-] Show Material materials with Hardness, Brinell of 75.0 [-] | T6 | EN 1706 | |
80.0 [-] Show Material materials with Hardness, Brinell of 80.0 [-] | T6 | EN 1706 | ||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | ||
Shear modulus | 2.8 GPa Show Material materials with Shear modulus of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | ||
Tensile strength | 220.0 MPa Show Material materials with Tensile strength of 220.0 MPa | T6 | EN 1706 | |
240.0 MPa Show Material materials with Tensile strength of 240.0 MPa | T6 | EN 1706 |
Thermal
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.1e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K | T6 | EN 1706 |
100 °C | 2.1e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.1e-05 1/K | T6 | EN 1706 | |
Melting point | 530.0 - 600.0 °C Show Material materials with Melting point of 530.0 - 600.0 °C | T6 | EN 1706 | |
Specific heat capacity | 900.0 J/(kg·K) Show Material materials with Specific heat capacity of 900.0 J/(kg·K) | T6 | EN 1706 | |
Thermal conductivity | 130.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 170.0 W/(m·K) | T6 | EN 1706 |
Electrical
Property | Value | Condition | Related Standards |
---|---|---|---|
Electrical conductivity | 16000000.0 - 24000000.0 S/m Show Material materials with Electrical conductivity of 16000000.0 - 24000000.0 S/m | T6 | EN 1706 |
Electrical resistivity | 4.17e-08 - 6.25e-08 Ω·m Show Material materials with Electrical resistivity of 4.17e-08 - 6.25e-08 Ω·m | T6 | EN 1706 |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Copper | 0.1 % Show Material materials with Copper of 0.1 % | T6 | EN 1706 |
Iron | 1.00 % Show Material materials with Iron of 1.00 % | T6 | EN 1706 |
Magnesium | 0.5 % Show Material materials with Magnesium of 0.5 % | T6 | EN 1706 |
Manganese | 0.001 - 0.4 % Show Material materials with Manganese of 0.001 - 0.4 % | T6 | EN 1706 |
Silicon | 9.0 - 11.0 % Show Material materials with Silicon of 9.0 - 11.0 % | T6 | EN 1706 |
Titanium | 0.15 % Show Material materials with Titanium of 0.15 % | T6 | EN 1706 |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | T6 | EN 1706 |
Technological properties
Property | ||
---|---|---|
Anodizing | decorative: not recommended | |
Corrosion properties | general: acceptable | |
General machinability | after thermal treatment: good to acceptable, as cast: good |