General
Property | Value | Comment |
---|---|---|
Density | 2.75 - 2.8 g/cm³ Show Material materials with Density of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mechanical
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium |
Melting point | 510.0 - 790.0 °C Show Material materials with Melting point of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium |
Specific heat capacity | 875.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium |
Thermal conductivity | 120.0 - 150.0 W/(m·K) Show Material materials with Thermal conductivity of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 16000000.0 - 23000000.0 S/m Show Material materials with Electrical conductivity of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Electrical resistivity | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Electrical resistivity of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 4.0 - 5.0 % Show Material materials with Copper of 4.0 - 5.0 % | Pink Sheets | Casting |
Iron | 0.07 % Show Material materials with Iron of 0.07 % | Pink Sheets | Casting |
Magnesium | 0.2 - 0.35 % Show Material materials with Magnesium of 0.2 - 0.35 % | Pink Sheets | Casting |
Manganese | 0.2 - 0.4 % Show Material materials with Manganese of 0.2 - 0.4 % | Pink Sheets | Casting |
Silicon | 0.05 % Show Material materials with Silicon of 0.05 % | Pink Sheets | Casting |
Silver | 0.4 - 1.0 % Show Material materials with Silver of 0.4 - 1.0 % | Pink Sheets | Casting |
Titanium | 0.15 - 0.35 % Show Material materials with Titanium of 0.15 - 0.35 % | Pink Sheets | Casting |