General
Property | Value | Comment |
---|---|---|
Density | 2.75 - 2.8 g/cm³ Show Material materials with Density of 2.75 - 2.8 g/cm³ | Typical for Cast 2xx.x Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 72.0 GPa Show Material materials with Elastic modulus of 72.0 GPa | Typical for Cast 2xx.x Series Aluminium | |||
Hardness, Brinell | 105.0 [-] Show Material materials with Hardness, Brinell of 105.0 [-] | T571 | Pink Sheets, ASTM B108 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | |||
Tensile strength | 235.0 MPa Show Material materials with Tensile strength of 235.0 MPa | T571 | Pink Sheets, ASTM B108 | Casting |
Thermal
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 1.9e-05 - 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.9e-05 - 2.3e-05 1/K | Typical for Cast 2xx.x Series Aluminium | |||
Melting point | 532.0 - 635.0 °C Show Material materials with Melting point of 532.0 - 635.0 °C | T571 | Pink Sheets, ASTM B108 | Casting | |
Specific heat capacity | 875.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium | |||
Thermal conductivity | 120.0 - 150.0 W/(m·K) Show Material materials with Thermal conductivity of 120.0 - 150.0 W/(m·K) | Typical for Cast 2xx.x Series Aluminium |
Electrical
Property | Value | Comment |
---|---|---|
Electrical conductivity | 16000000.0 - 23000000.0 S/m Show Material materials with Electrical conductivity of 16000000.0 - 23000000.0 S/m | Typical for Cast 2xx.x Series Aluminium |
Electrical resistivity | 4.347826086956522e-08 - 6.25e-08 Ω·m Show Material materials with Electrical resistivity of 4.347826086956522e-08 - 6.25e-08 Ω·m | Typical for Cast 2xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Chromium | 0.25 % Show Material materials with Chromium of 0.25 % | T571 | Pink Sheets, ASTM B108 | Casting |
Copper | 3.5 - 4.5 % Show Material materials with Copper of 3.5 - 4.5 % | T571 | Pink Sheets, ASTM B108 | Casting |
Iron | 1.00 % Show Material materials with Iron of 1.00 % | T571 | Pink Sheets, ASTM B108 | Casting |
Magnesium | 1.2 - 1.8 % Show Material materials with Magnesium of 1.2 - 1.8 % | T571 | Pink Sheets, ASTM B108 | Casting |
Manganese | 0.35 % Show Material materials with Manganese of 0.35 % | T571 | Pink Sheets, ASTM B108 | Casting |
Nickel | 1.7 - 2.3 % Show Material materials with Nickel of 1.7 - 2.3 % | T571 | Pink Sheets, ASTM B108 | Casting |
Silicon | 0.7 % Show Material materials with Silicon of 0.7 % | T571 | Pink Sheets, ASTM B108 | Casting |
Titanium | 0.25 % Show Material materials with Titanium of 0.25 % | T571 | Pink Sheets, ASTM B108 | Casting |
Zinc | 0.35 % Show Material materials with Zinc of 0.35 % | T571 | Pink Sheets, ASTM B108 | Casting |