General
Property | Value | Comment |
---|---|---|
Density | 2.65 - 2.7 g/cm³ Show Material materials with Density of 2.65 - 2.7 g/cm³ | Typical for Cast 3xx.x Series Aluminium |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 73.0 - 80.0 GPa Show Material materials with Elastic modulus of 73.0 - 80.0 GPa | Typical for Cast 3xx.x Series Aluminium |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium |
Shear modulus | 2.8 GPa Show Material materials with Shear modulus of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium |
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium |
Melting point | 505.0 - 770.0 °C Show Material materials with Melting point of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Specific heat capacity | 960.0 - 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Thermal conductivity | 130.0 - 180.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 0.7 - 1.1 % Show Material materials with Copper of 0.7 - 1.1 % | Pink Sheets | Casting |
Iron | 1.00 % Show Material materials with Iron of 1.00 % | Pink Sheets | Casting |
Magnesium | 0.8 - 1.3 % Show Material materials with Magnesium of 0.8 - 1.3 % | Pink Sheets | Casting |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | Pink Sheets | Casting |
Nickel | 2.0 - 2.5 % Show Material materials with Nickel of 2.0 - 2.5 % | Pink Sheets | Casting |
Silicon | 21.0 - 23.0 % Show Material materials with Silicon of 21.0 - 23.0 % | Pink Sheets | Casting |
Titanium | 0.1 - 0.2 % Show Material materials with Titanium of 0.1 - 0.2 % | Pink Sheets | Casting |
Vanadium | 0.08 - 0.15 % Show Material materials with Vanadium of 0.08 - 0.15 % | Pink Sheets | Casting |
Zinc | 0.1 % Show Material materials with Zinc of 0.1 % | Pink Sheets | Casting |