Property | Value | Comment |
---|---|---|
Density | 2.65 - 2.71 g/cm³ Show Material materials with Density of 2.65 - 2.71 g/cm³ | Typical for Cast 4xx.x Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Bending Fatigue Strength | 130.0 MPa Show Material materials with Bending Fatigue Strength of 130.0 MPa | F | Pink Sheets, ASTM B85 | Casting | |
Elastic modulus | 71.0 - 75.0 GPa Show Material materials with Elastic modulus of 71.0 - 75.0 GPa | Typical for Cast 4xx.x Series Aluminium | |||
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 4xx.x Series Aluminium | |||
Tensile strength | 295.0 MPa Show Material materials with Tensile strength of 295.0 MPa | F | Pink Sheets, ASTM B85 | Casting |
Thermal
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2e-05 - 2.2e-05 1/K Show Material materials with Coefficient of thermal expansion of 2e-05 - 2.2e-05 1/K | Typical for Cast 4xx.x Series Aluminium | |||
Melting point | 574.0 - 582.0 °C Show Material materials with Melting point of 574.0 - 582.0 °C | F | Pink Sheets, ASTM B85 | Casting | |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 4xx.x Series Aluminium | |||
Thermal conductivity | 130.0 - 170.0 W/(m·K) Show Material materials with Thermal conductivity of 130.0 - 170.0 W/(m·K) | Typical for Cast 4xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 1.0 % Show Material materials with Copper of 1.0 % | F | Pink Sheets, ASTM B85 | Casting |
Iron | 2.00 % Show Material materials with Iron of 2.00 % | F | Pink Sheets, ASTM B85 | Casting |
Magnesium | 0.1 % Show Material materials with Magnesium of 0.1 % | F | Pink Sheets, ASTM B85 | Casting |
Manganese | 0.35 % Show Material materials with Manganese of 0.35 % | F | Pink Sheets, ASTM B85 | Casting |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % | F | Pink Sheets, ASTM B85 | Casting |
Silicon | 11.0 - 13.0 % Show Material materials with Silicon of 11.0 - 13.0 % | F | Pink Sheets, ASTM B85 | Casting |
Tin | 0.15 % Show Material materials with Tin of 0.15 % | F | Pink Sheets, ASTM B85 | Casting |
Zinc | 0.5 % Show Material materials with Zinc of 0.5 % | F | Pink Sheets, ASTM B85 | Casting |