General
Property | Value | Comment |
---|---|---|
Density | 2.6 - 2.7 g/cm³ Show Material materials with Density of 2.6 - 2.7 g/cm³ | Typical for Cast 5xx.x Series Aluminium |
Mechanical
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elastic modulus | 68.0 - 70.0 GPa Show Material materials with Elastic modulus of 68.0 - 70.0 GPa | Typical for Cast 5xx.x Series Aluminium | |||
Hardness, Brinell | 60.0 [-] Show Material materials with Hardness, Brinell of 60.0 [-] | F | Pink Sheets, ASTM B108 | Casting | |
Poisson's ratio | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Cast 5xx.x Series Aluminium | |||
Tensile strength | 150.0 MPa Show Material materials with Tensile strength of 150.0 MPa | F | Pink Sheets, ASTM B108 | Casting |
Thermal
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Coefficient of thermal expansion | 2.3e-05 - 2.5e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 - 2.5e-05 1/K | Typical for Cast 5xx.x Series Aluminium | |||
Melting point | 579.0 - 638.0 °C Show Material materials with Melting point of 579.0 - 638.0 °C | F | Pink Sheets, ASTM B108 | Casting | |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 5xx.x Series Aluminium | |||
Thermal conductivity | 60.0 - 140.0 W/(m·K) Show Material materials with Thermal conductivity of 60.0 - 140.0 W/(m·K) | Typical for Cast 5xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Copper | 0.1 % Show Material materials with Copper of 0.1 % | F | Pink Sheets, ASTM B108 | Casting |
Iron | 0.40 % Show Material materials with Iron of 0.40 % | F | Pink Sheets, ASTM B108 | Casting |
Magnesium | 3.5 - 4.5 % Show Material materials with Magnesium of 3.5 - 4.5 % | F | Pink Sheets, ASTM B108 | Casting |
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % | F | Pink Sheets, ASTM B108 | Casting |
Silicon | 0.3 % Show Material materials with Silicon of 0.3 % | F | Pink Sheets, ASTM B108 | Casting |
Titanium | 0.2 % Show Material materials with Titanium of 0.2 % | F | Pink Sheets, ASTM B108 | Casting |
Zinc | 1.4 - 2.2 % Show Material materials with Zinc of 1.4 - 2.2 % | F | Pink Sheets, ASTM B108 | Casting |