General
Property | Value | Comment |
---|---|---|
Density | 2.8 g/cm³ Show Material materials with Density of 2.8 g/cm³ | Typical for Cast 8xx.x Series Aluminium |
Mechanical
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 2.3e-05 1/K Show Material materials with Coefficient of thermal expansion of 2.3e-05 1/K | Typical for Cast 8xx.x Series Aluminium |
Melting point | 205.0 - 650.0 °C Show Material materials with Melting point of 205.0 - 650.0 °C | Typical for Cast 8xx.x Series Aluminium |
Specific heat capacity | 963.0 J/(kg·K) Show Material materials with Specific heat capacity of 963.0 J/(kg·K) | Typical for Cast 8xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards | Shape |
---|---|---|---|
Copper | 1.7 - 2.3 % Show Material materials with Copper of 1.7 - 2.3 % | Pink Sheets | Casting |
Iron | 0.50 % Show Material materials with Iron of 0.50 % | Pink Sheets | Casting |
Magnesium | 0.7 - 0.9 % Show Material materials with Magnesium of 0.7 - 0.9 % | Pink Sheets | Casting |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | Pink Sheets | Casting |
Nickel | 0.9 - 1.5 % Show Material materials with Nickel of 0.9 - 1.5 % | Pink Sheets | Casting |
Silicon | 0.4 % Show Material materials with Silicon of 0.4 % | Pink Sheets | Casting |
Tin | 5.5 - 7.0 % Show Material materials with Tin of 5.5 - 7.0 % | Pink Sheets | Casting |
Titanium | 0.2 % Show Material materials with Titanium of 0.2 % | Pink Sheets | Casting |