General
Property | Value | Comment |
---|---|---|
Density | 2.75 g/cm³ Show Material materials with Density of 2.75 g/cm³ | Typical for Cast 1xx.x Series Aluminium |
Mechanical
Thermal
Property | Value | Comment |
---|---|---|
Coefficient of thermal expansion | 1.8e-05 - 2.4e-05 1/K Show Material materials with Coefficient of thermal expansion of 1.8e-05 - 2.4e-05 1/K | Typical for Cast 1xx.x Series Aluminium |
Melting point | 643.0 - 657.0 °C Show Material materials with Melting point of 643.0 - 657.0 °C | Typical for Cast 1xx.x Series Aluminium |
Thermal conductivity | 209.0 - 222.0 W/(m·K) Show Material materials with Thermal conductivity of 209.0 - 222.0 W/(m·K) | Typical for Cast 1xx.x Series Aluminium |
Chemical properties
Property | Value | Related Standards |
---|---|---|
Arsenic | 0.009 % Show Material materials with Arsenic of 0.009 % | Gold Sheets |
Gallium | 0.04 % Show Material materials with Gallium of 0.04 % | Gold Sheets |
Iron | 0.55 % Show Material materials with Iron of 0.55 % | Gold Sheets |
Silicon | 0.2 % Show Material materials with Silicon of 0.2 % | Gold Sheets |
Vanadium | 0.04 % Show Material materials with Vanadium of 0.04 % | Gold Sheets |
Zinc | 0.03 % Show Material materials with Zinc of 0.03 % | Gold Sheets |