Chemical properties
Property | Value | Related Standards |
---|---|---|
Calcium | 0.5 % Show Material materials with Calcium of 0.5 % | Gold Sheets |
Chromium | 0.05 % Show Material materials with Chromium of 0.05 % | Gold Sheets |
Copper | 0.05 % Show Material materials with Copper of 0.05 % | Gold Sheets |
Iron | 1.50 % Show Material materials with Iron of 1.50 % | Gold Sheets |
Manganese | 0.1 % Show Material materials with Manganese of 0.1 % | Gold Sheets |
Nickel | 0.05 % Show Material materials with Nickel of 0.05 % | Gold Sheets |
Phosphorus | 0.01 % Show Material materials with Phosphorus of 0.01 % | Gold Sheets |
Silicon | 12.0 - 16.0 % Show Material materials with Silicon of 12.0 - 16.0 % | Gold Sheets |
Strontium | 9.0 - 11.0 % Show Material materials with Strontium of 9.0 - 11.0 % | Gold Sheets |
Titanium | 0.1 % Show Material materials with Titanium of 0.1 % | Gold Sheets |
Vanadium | 0.05 % Show Material materials with Vanadium of 0.05 % | Gold Sheets |
Zirconium | 0.1 % Show Material materials with Zirconium of 0.1 % | Gold Sheets |