JIS H2102 Class 3

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueComment

Density

2.75 g/cm³

Show Material materials with Density of 2.75 g/cm³

Typical for Cast 1xx.x Series Aluminium

Mechanical

PropertyValueComment

Elastic modulus

70.0 GPa

Show Material materials with Elastic modulus of 70.0 GPa

Typical for Cast 1xx.x Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Cast 1xx.x Series Aluminium

Thermal

PropertyValueComment

Coefficient of thermal expansion

1.8e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 1.8e-05 - 2.4e-05 1/K

Typical for Cast 1xx.x Series Aluminium

Melting point

643.0 - 657.0 °C

Show Material materials with Melting point of 643.0 - 657.0 °C

Typical for Cast 1xx.x Series Aluminium

Thermal conductivity

209.0 - 222.0 W/(m·K)

Show Material materials with Thermal conductivity of 209.0 - 222.0 W/(m·K)

Typical for Cast 1xx.x Series Aluminium

Chemical properties

PropertyValueRelated Standards

Aluminium

99.0 %

Show Material materials with Aluminium of 99.0 %

JIS H2102

Copper

0.02 %

Show Material materials with Copper of 0.02 %

JIS H2102

Iron

0.80 %

Show Material materials with Iron of 0.80 %

JIS H2102

Manganese

0.03 %

Show Material materials with Manganese of 0.03 %

JIS H2102

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

JIS H2102

Titanium

0.03 %

Show Material materials with Titanium of 0.03 %

JIS H2102