Description

The exceptional wear and fatigue resistance of this alloy results from a controlled duplex alpha and beta phase. This alloy has high strength combined with good ductility and unusual toughness. The physical characteristics of this alloy can be varied by heat treatments (AMPCO® 18.22, 18.23 and 18.136).

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.45 g/cm³

Show Supplier Material materials with Density of 7.45 g/cm³

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

32 J

Show Supplier Material materials with Charpy impact energy of 32 J

Compressive strength

23.0 °C

990 MPa

Show Supplier Material materials with Compressive strength of 990 MPa

Elastic modulus

23.0 °C

115 GPa

Show Supplier Material materials with Elastic modulus of 115 GPa

Elongation A5

23.0 °C

15 %

Show Supplier Material materials with Elongation A5 of 15 %

Fatigue strength

23.0 °C

240 MPa

Show Supplier Material materials with Fatigue strength of 240 MPa

100.000.000 cycles

Hardness, HBW

23.0 °C

187 [-]

Show Supplier Material materials with Hardness, HBW of 187 [-]

HBW 10/3000

Hardness, Rockwell B

23.0 °C

91 [-]

Show Supplier Material materials with Hardness, Rockwell B of 91 [-]

Izod impact energy

23.0 °C

30 J

Show Supplier Material materials with Izod impact energy of 30 J

Proportional limit in compression

23.0 °C

230 MPa

Show Supplier Material materials with Proportional limit in compression of 230 MPa

Reduction of area

23.0 °C

14 %

Show Supplier Material materials with Reduction of area of 14 %

Shear strength

23.0 °C

420 MPa

Show Supplier Material materials with Shear strength of 420 MPa

Tensile strength

23.0 °C

724 MPa

Show Supplier Material materials with Tensile strength of 724 MPa

Yield strength Rp0.5

23.0 °C

296 MPa

Show Supplier Material materials with Yield strength Rp0.5 of 296 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.62E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-5 1/K

Specific heat capacity

23.0 °C

420 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K)

Thermal conductivity

23.0 °C

63 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 63 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

8.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 8.00E+6 S/m

Specific Electrical conductivity

14 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 14 % IACS

Chemical properties

PropertyValue

Aluminium

10.5 %

Show Supplier Material materials with Aluminium of 10.5 %

Copper

Balance

Iron

3.5 %

Show Supplier Material materials with Iron of 3.5 %

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

Technological properties

Property
Application areas

This alloy is well suited for use as gears, worm wheels, bushings and bearings. The machine tool industry has adopted AMPCO® 18 as standard for all applications requiring good sliding properties, wear resistance, fatigue resistance, toughness and/or resistance to deformation under load. AMPCO® 18 is used in steel mill service as screw down nuts, slippers (many of which are "cast to size"), gears, wedges and breaker blocks. AMPCO® 18 has an excellent corrosion resistance and is used in pickling service for such parts as hooks, crates and spreaders, etc.