AMPCO® 26 Sand castings

Want to keep this datasheet? Save it now in your required format

Description

AMPCO® 26 is a patented hard grade aluminium bronze. Its exceptional hardness makes it a unique material. However, this extreme hardness means fragility and machinability difficulties. This alloy has very limited uses and machinability, but it gives exceptional results.

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

6.84 g/cm³

Show Supplier Material materials with Density of 6.84 g/cm³

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Compressive strength

23.0 °C

1515 MPa

Show Supplier Material materials with Compressive strength of 1515 MPa

Compressive yield strength, 0.1%

23.0 °C

689 MPa

Show Supplier Material materials with Compressive yield strength, 0.1% of 689 MPa

Hardness, HBW

23.0 °C

418 [-]

Show Supplier Material materials with Hardness, HBW of 418 [-]

HBW 10/3000

Hardness, Rockwell C

23.0 °C

43 [-]

Show Supplier Material materials with Hardness, Rockwell C of 43 [-]

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

23.0 °C

1.6E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.6E-5 1/K

Specific heat capacity

23.0 °C

420 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K)

Thermal conductivity

23.0 °C

33 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 33 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

4.00E+6 S/m

Show Supplier Material materials with Electrical conductivity of 4.00E+6 S/m

Specific Electrical conductivity

8 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 8 % IACS

Chemical properties

PropertyValue

Copper

Balance

Technological properties

Property
Application areas

Stainless steel drawing dies, forming rolls under great stresses and extreme pressures are the most typical applications for this alloy.