AMPCO-TRODE® 40 Bare

Alternative and trade names
AWS A5.7 Class E CuMnNiAl, ASME SFA 5.7 Class E CuMnNiAl
Want to keep this datasheet? Save it now in your required format

Description

AMPCO-TRODE® 40 manganese-nickel-aluminum bronze is available in coated electrodes, bare filler metal rod and wire for welding cast ship propellers conforming to MIL-B-21230, Alloy 2 for high resistance to corrosion, erosion and cavitation.


AMPCO-TRODE® 40 also exhibits good ability to join dissimilar metals.

Related Standards

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

27 %

Show Supplier Material materials with Elongation of 27 %

in 2″ (51 mm)

Hardness, Brinell

23.0 °C

217 [-]

Show Supplier Material materials with Hardness, Brinell of 217 [-]

BHN (3000kg) 1/4″ (6.4mm) deposit

Reduction of area

23.0 °C

37 %

Show Supplier Material materials with Reduction of area of 37 %

Tensile strength

23.0 °C

759 MPa

Show Supplier Material materials with Tensile strength of 759 MPa

Yield strength

23.0 °C

462 MPa

Show Supplier Material materials with Yield strength of 462 MPa

Chemical properties

PropertyValueComment

Aluminium

7 - 8.5 %

Show Supplier Material materials with Aluminium of 7 - 8.5 %

Copper

Balance, including silver

Iron

2 - 4 %

Show Supplier Material materials with Iron of 2 - 4 %

Manganese

11 - 14 %

Show Supplier Material materials with Manganese of 11 - 14 %

Nickel

1.5 - 3 %

Show Supplier Material materials with Nickel of 1.5 - 3 %

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max.

Silicon

1.5 %

Show Supplier Material materials with Silicon of 1.5 %

max.

Technological properties

Property
Application areas

Welding: Ship propellers, Marine components, Welding cast iron, Joining dissimilar metals