Description

AMPCO-TRODE® 46 nickel-aluminum bronze spooled wire, bare rod and coated electrodes were developed for the welding of the cast and wrought nickel-aluminum bronze.


AMPCO-TRODE® 46 is also recommended for weld repairing NiBral boat propellers.

Related Standards

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

23 %

Show Supplier Material materials with Elongation of 23 %

in 2″ (51 mm)

Hardness, Brinell

23.0 °C

196 [-]

Show Supplier Material materials with Hardness, Brinell of 196 [-]

BHN (3000kg) 1/4″ (6.4mm) deposit

Reduction of area

23.0 °C

22 %

Show Supplier Material materials with Reduction of area of 22 %

Tensile strength

23.0 °C

718 MPa

Show Supplier Material materials with Tensile strength of 718 MPa

Yield strength

23.0 °C

407 MPa

Show Supplier Material materials with Yield strength of 407 MPa

Chemical properties

PropertyValueComment

Aluminium

8.5 - 9.5 %

Show Supplier Material materials with Aluminium of 8.5 - 9.5 %

Copper

Balance, including silver

Iron

3 - 5 %

Show Supplier Material materials with Iron of 3 - 5 %

Manganese

0.6 - 3.5 %

Show Supplier Material materials with Manganese of 0.6 - 3.5 %

Nickel

4 - 5.5 %

Show Supplier Material materials with Nickel of 4 - 5.5 %

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max.

Silicon

0.1 %

Show Supplier Material materials with Silicon of 0.1 %

max.

Technological properties

Property