AMPCO-TRODE® 521

Alternative and trade names
AWS A5.7 Class ER CuAl-A1, ASME SFA 5.7 Class ER CuAl-A1
Want to keep this datasheet? Save it now in your required format

Description

Base materials: Particularly suitable for high stressed corrosion resistant weld surfacing on cast iron and on unalloyed and low- alloyed steel as well as seawater resistant CuZn alloys. Suitable for welding on CuNi.


Shielding gas: Argon, Helium or Argon/Helium-mixtures

Related Standards

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

47 %

Show Supplier Material materials with Elongation of 47 %

in 2″ (51 mm)

Hardness, Brinell

23.0 °C

125 [-]

Show Supplier Material materials with Hardness, Brinell of 125 [-]

BHN (3000kg) 1/4″ (6.4mm) deposit

Reduction of area

23.0 °C

53 %

Show Supplier Material materials with Reduction of area of 53 %

Tensile strength

23.0 °C

469 MPa

Show Supplier Material materials with Tensile strength of 469 MPa

Yield strength

23.0 °C

193 MPa

Show Supplier Material materials with Yield strength of 193 MPa

Chemical properties

PropertyValueComment

Aluminium

6 - 8.5 %

Show Supplier Material materials with Aluminium of 6 - 8.5 %

Copper

Balance, including silver

Manganese

0.5 %

Show Supplier Material materials with Manganese of 0.5 %

max.

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max.

Silicon

0.1 %

Show Supplier Material materials with Silicon of 0.1 %

max.

Technological properties

Property
Application areas

Welding: Tube sheets, Pickling hooks, Impellers valve seats, Chemical plants, Pulp mills