Description

COPR-TRODE® is a deoxidized copper alloy developed to provide dense, high quality deposits with relatively high electrical conductivity for use in joining and overlay with the inert-gas processes.


COPR-TRODE® spooled wire and filler metal rod are used primarily to fabricate deoxidized copper and repair weld copper castings with the gas metal-arc and gas tungsten-arc processes. It may also be used to weld galvanized steel and deoxidized copper to mild steel where high strength joints are not required.


COPR-TRODE® spooled wire and filler metal rod are used to overlay surfaces to resist corrosion.

Equivalent Materials

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

29 %

Show Supplier Material materials with Elongation of 29 %

in 2″ (51 mm)

Hardness, Brinell

23.0 °C

54 [-]

Show Supplier Material materials with Hardness, Brinell of 54 [-]

BHN (3000kg) 1/4″ (6.4mm) deposit

Reduction of area

23.0 °C

45 %

Show Supplier Material materials with Reduction of area of 45 %

Tensile strength

23.0 °C

200 MPa

Show Supplier Material materials with Tensile strength of 200 MPa

Yield strength

23.0 °C

55 MPa

Show Supplier Material materials with Yield strength of 55 MPa

Electrical

PropertyValue

Specific Electrical conductivity

40 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 40 % IACS

Chemical properties

PropertyValueComment

Copper

Balance, including silver

Manganese

0.5 %

Show Supplier Material materials with Manganese of 0.5 %

max.

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max.

Phosphorus

0.15 %

Show Supplier Material materials with Phosphorus of 0.15 %

max.

Silicon

0.5 %

Show Supplier Material materials with Silicon of 0.5 %

max.

Tin

1 %

Show Supplier Material materials with Tin of 1 %

max.

Technological properties

Property
Application areas

Welding: Billet molds, Conductor rolls, Heater elements, Copper sculptures, Steel mill electrode holders, Bus bars, Copper connectors