KOLCHUGA PFCG

Alternative and trade names
KOLCHUGA PFCG
Want to keep this datasheet? Save it now in your required format

Description

A protective fiber glass coating (hereinafter referred to as PFC) for steel pipes and bends with an outer diameter of 219 to 1420 mm, designed to protect the pipelines corrosion-resistant coating from mechanical damage during construction, reconstruction, repair and during operation. By designation, PFC is applied to the pipe in two versions: general “G” or reinforced “R”.

This material data has been provided by METACLAY .

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.45 - 1.75 g/cm³

Show Supplier Material materials with Density of 1.45 - 1.75 g/cm³

GOST 15139-69

Mechanical

PropertyTemperatureValueComment

Charpy impact energy

23.0 °C

150 J

Show Supplier Material materials with Charpy impact energy of 150 J

Min.

Flexural strength

23.0 °C

136 MPa

Show Supplier Material materials with Flexural strength of 136 MPa

Min., ISO 14125:1998

Tensile strength

23.0 °C

500 MPa

Show Supplier Material materials with Tensile strength of 500 MPa

Min., ISO 527-5/Tape

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.5E-5 - 2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.5E-5 - 2.4E-5 1/K

GOST 15173-70

Specific heat capacity

23.0 °C

900 - 1300 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 900 - 1300 J/(kg·K)

GOST Р 57712-2017

Thermal conductivity

23.0 °C

0.3 - 0.4 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 0.3 - 0.4 W/(m·K)

GOST Р 57830-2017

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.50E+18 Ω·m

Show Supplier Material materials with Electrical resistivity of 1.50E+18 Ω·m

GOST 6433.2-71

Technological properties

Property
Application areas

KOLCHUGA PFCG is designated to protect the pipelines and bends insulation coating from mechanical damage when they are laid by trench method in rocky and permafrost soils, including backfill soil which contains inclusions of gruss, flint, pebbles, spalls and larger solid inclusions.

Fillers

Glass Fiber