Arnitel® EL430

Alternative and trade names
TPC-ET
Want to keep this datasheet? Save it now in your required format

Description

Arnitel® is a high-performance ThermoPlastic Copolyester (TPC) that offers you a unique combination of flexibility, high temperature resistance and strength - plus excellent processing characteristics.
In industries ranging from automotive to E&E, Arnitel® is increasingly being as a lighter, smarter, greener alternative to conventional rubbers – reducing environmental impact and ultimately, system costs.
The product is supported by an experienced and knowledgeable global team continuously working on new ideas and applications, as well as exploring new markets. By listening to your needs and understanding your process and products, we develop solutions that make a real difference.

Datasheet URL:

Arnitel® EL430

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

dry

ISO 1183

Mechanical

PropertyValueConditionTesting StandardComment

Elastic modulus

0.05 GPa

Show Supplier Material materials with Elastic modulus of 0.05 GPa

dry

ISO 527-1/-2

Elongation

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

50 %

Show Supplier Material materials with Elongation of 50 %

dry

ISO 527-1/-2

Hardness, Shore A

92 [-]

Show Supplier Material materials with Hardness, Shore A of 92 [-]

dry

ISO 868

3s

Hardness, Shore D

33 [-]

Show Supplier Material materials with Hardness, Shore D of 33 [-]

dry

ISO 868

3s

Tensile strength

18 MPa

Show Supplier Material materials with Tensile strength of 18 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardComment

Glass transition temperature

-58.0 °C

Show Supplier Material materials with Glass transition temperature of -58.0 °C

dry

ASTM D5026/D7028

DMTA (tan d)

Melting point

160 °C

Show Supplier Material materials with Melting point of 160 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyTemperatureValueConditionTesting Standard

Melt volume-flow rate

230 °C

33 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 33 cm³/10min

dry

ISO 1133

Technological properties

Property
Certifications

Food Contact