Novamid® 1010GH30 NAT

Alternative and trade names
PA6-GF30
Want to keep this datasheet? Save it now in your required format

Description

Novamid® is a high-quality polyamide, that has been developed as a special product line in order to cope with high demand levels from our Japanese customers.
Novamid® has seen various applications in various fields and various regions. From car to packaging, Novamid® is supported by an experienced and wide range of experts.

Datasheet URL:

Novamid® 1010GH30 NAT

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionTesting Standard

Density

1.36 g/cm³

Show Supplier Material materials with Density of 1.36 g/cm³

dry

ISO 1183

Moisture absorption

2 %

Show Supplier Material materials with Moisture absorption of 2 %

dry

Sim. to ISO 62

Mechanical

PropertyTemperatureValueConditionTesting Standard

Elastic modulus

5.7 GPa

Show Supplier Material materials with Elastic modulus of 5.7 GPa

conditioned

ISO 527-1/-2

9.6 GPa

Show Supplier Material materials with Elastic modulus of 9.6 GPa

dry

ISO 527-1/-2

Elongation

3.3 %

Show Supplier Material materials with Elongation of 3.3 %

dry

ISO 527-1/-2

5.6 %

Show Supplier Material materials with Elongation of 5.6 %

conditioned

ISO 527-1/-2

Flexural modulus

5.6 GPa

Show Supplier Material materials with Flexural modulus of 5.6 GPa

conditioned

ISO 178

9.2 GPa

Show Supplier Material materials with Flexural modulus of 9.2 GPa

dry

ISO 178

Flexural yield strength

165 MPa

Show Supplier Material materials with Flexural yield strength of 165 MPa

conditioned

ISO 178

260 MPa

Show Supplier Material materials with Flexural yield strength of 260 MPa

dry

ISO 178

Impact strength, Charpy notched

23 °C

12 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 12 kJ/m²

dry

ISO 179/1eA

23 °C

19 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 19 kJ/m²

conditioned

ISO 179/1eA

Impact strength, Charpy unnotched

23 °C

81 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 81 kJ/m²

dry

ISO 179/1eU

23 °C

92 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 92 kJ/m²

conditioned

ISO 179/1eU

Unlock all property charts

Tensile strength

110 MPa

Show Supplier Material materials with Tensile strength of 110 MPa

conditioned

ISO 527-1/-2

170 MPa

Show Supplier Material materials with Tensile strength of 170 MPa

dry

ISO 527-1/-2

Thermal

PropertyValueConditionTesting StandardPressureComment

Coefficient of thermal expansion

3e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 3e-07 1/K

dry

ISO 11359-1/-2

Parallel

7e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 7e-07 1/K

dry

ISO 11359-1/-2

Normal

Heat deflection temperature

205 °C

Show Supplier Material materials with Heat deflection temperature of 205 °C

dry

ISO 75-1/-2

2 MPa

220 °C

Show Supplier Material materials with Heat deflection temperature of 220 °C

dry

ISO 75-1/-2

0.45 MPa

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Electrical

PropertyValueConditionTesting Standard

Surface resistivity

2e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 2e+14 Ω/sq

conditioned

IEC 62631-3-2

Rheological Properties

PropertyTemperatureValueConditionTesting StandardComment

Melt volume-flow rate

250 °C

31 cm³/10min

Show Supplier Material materials with Melt volume-flow rate of 31 cm³/10min

dry

ISO 1133

Shrinkage

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

dry

ISO 294-4

Parallel

1 %

Show Supplier Material materials with Shrinkage of 1 %

dry

ISO 294-4

Normal

Technological properties

Property
Fillers

30% Glass Fiber