Akulon® F-X9182

Want to keep this datasheet? Save it now in your required format

Description

Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® F-X9182

This material data has been provided by DSM.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueConditionTesting Standard

Density

1.13 g/cm³

Show Supplier Material materials with Density of 1.13 g/cm³

dry

ISO 1183

Moisture absorption

2.5 %

Show Supplier Material materials with Moisture absorption of 2.5 %

dry

Sim. to ISO 62

Water absorption

9.5 %

Show Supplier Material materials with Water absorption of 9.5 %

dry

Sim. to ISO 62

Thermal

PropertyValueConditionTesting StandardComment

Coefficient of thermal expansion

9e-07 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 9e-07 1/K

dry

ISO 11359-1/-2

Parallel

1e-06 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1e-06 1/K

dry

ISO 11359-1/-2

Normal

Melting point

220 °C

Show Supplier Material materials with Melting point of 220 °C

dry

ISO 11357-1/-3

10°C/min

Rheological Properties

PropertyValueConditionTesting Standard

Viscosity number

160 cm³/gr

Show Supplier Material materials with Viscosity number of 160 cm³/gr

dry

ISO 307, 1157, 1628

Technological properties

Property
Certifications

Food Contact