Flame retardant epoxy moulding compound with good mechanical properties, excellent chemical and high tracking resistance. Flame retardancy (d = 1.5mm) Class V-0. Shelf life: 12 months at temperatures below 8°C.
See where Epoxy NU 514 K/L falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ1.9 g/cm³ at 20 °C
DIN 53479
Water absorption
cwater0.06 % at 20 °C
ISO 62, 100°C/30 min
Coefficient of thermal expansion
α2.5E-5 1/K at 20 °C
ISO 11359-2, Mean value for 20-105°C
Glass transition temperature
Tg160 °C
ISO 6721
Thermal conductivity
λ0.7 W/(m·K) at 20 °C
ISO 8894
Comparative tracking index
CTI600 V at 20 °C
IEC 60112
Dielectric constant, 50Hz
εr,50Hz5.6 [-] at 20 °C
IEC 60250
Dielectric strength
EDS22 kV/mm at 20 °C
IEC 60243-1, 3mm Plate
Electrical resistivity
ρel1.00E+11 Ω·m at 20 °C
IEC 60093
Loss tangent, 50Hz
tanδ50,Hz2 [-] at 20 °C
IEC 60250
Application areas
Electro insulation material for Bushings, Connectors, Ex-proof applications, Insulators, Switches. Suitable also for applications with high radiation exposure
This material data has been provided by Duresco GmbH.