Glass fibre reinforced epoxy moulding compound with high latency for multi-purpose applications with Shelf life of 18 months at temperatures ≤ 8°C 6 months at temperatures ≤18°C
See where Epoxy NU 5680 V falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ2 g/cm³ at 20 °C
DIN 53479
Water absorption
cwater0.1 % at 20 °C
ISO 62, 100°C/30 min
Coefficient of thermal expansion
α2E-5 1/K at 20 °C
ISO 11359-2, Mean value for 20-105°C
Glass transition temperature
Tg165 °C
ISO 6721-7
Thermal conductivity
λ1 W/(m·K) at 20 °C
ISO 8894
Comparative tracking index
CTI250 V at 20 °C
IEC 60112
Dielectric constant, 50Hz
εr,50Hz5.2 [-] at 20 °C
IEC 60250
Dielectric strength
EDS23 kV/mm at 20 °C
IEC 60243-1, 3mm Plate
Electrical resistivity
ρel1.00E+12 Ω·m at 20 °C
IEC 60093
Loss tangent, 50Hz
tanδ50,Hz1.8 [-] at 20 °C
IEC 60250
Application areas
Encapsulation of electrical devices e.g. Solenoids, Sensors, Electronics
Fillers
Glass Fiber