Description

Eplamid 66 Impact modified compounds are used in all sectors of industry, offering a good impact strength for mechanical properties and ensures an outstanding performance even at low temperatures (up to -40°C). This material is available in natural and colours on request.

This material data has been provided by Epsan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.12 g/cm³

Show Supplier Material materials with Density of 1.12 g/cm³

ISO 1183

Water content

23.0 °C

0.1 %

Show Supplier Material materials with Water content of 0.1 %

ISO 15512

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.8 GPa

Show Supplier Material materials with Elastic modulus of 2.8 GPa

ISO 527-2 (1mm/min)

Elongation

23.0 °C

40 %

Show Supplier Material materials with Elongation of 40 %

min., ISO 527-2 (5mm/min)

Flexural modulus

23.0 °C

2.3 GPa

Show Supplier Material materials with Flexural modulus of 2.3 GPa

ISO 178 (2mm/min)

Flexural strength

23.0 °C

90 MPa

Show Supplier Material materials with Flexural strength of 90 MPa

ISO 178 (2mm/min)

Impact strength, Charpy notched

-30.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m²

ISO 179/1eA

23.0 °C

15 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 15 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-40.0 °C

10 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m²

ISO 180/1A

23.0 °C

13 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 13 kJ/m²

ISO 180/1A

Unlock all property charts

Tensile strength

23.0 °C

60 MPa

Show Supplier Material materials with Tensile strength of 60 MPa

ISO 527-2 (5mm/min)

Impact strength, Charpy unnotched

no break at 23°C; ISO 179/1eU

Impact strength, Izod unnotched

no break at 23°C; ISO 180/1U

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

190 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 190 °C

ISO 75-2/B

Heat deflection temperature, 1.80 MPa

95 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 95 °C

ISO 75-2/A

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 3146

Flammability

UL94 (0.8mm) HB

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

EN 60112

Surface resistivity

23.0 °C

1.00E+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+14 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1.6 %

Show Supplier Material materials with Shrinkage of 1.6 %

ISO 294-4 (3mm)

Shrinkage, transverse

23.0 °C

2 %

Show Supplier Material materials with Shrinkage, transverse of 2 %

ISO 294-4 (3mm)

Technological properties

Property
Application areas

Halogen free based on red phosphorus flame retardant grades, compliance with RoHS derivatives, with rating UL94 V0 and glow-wire at 960°C, which is used in many sectors of industy and has excellent mechanical properties.

Certifications

RoHS

Other