Description

Unreinforced and modified polyamide 66 improved with good-impact resistance, heat stabilized and lubricated for injection molding.

Eplamid 66 Impact modified compounds are used in all sectors of industry, offering a good impact strength for mechanical properties and ensures an outstanding performance even at low temperatures (up to -40°C).

This material is available in natural and colours on request.

This material data has been provided by Epsan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.08 g/cm³

Show Supplier Material materials with Density of 1.08 g/cm³

ISO 1183

Water content

23.0 °C

0.1 %

Show Supplier Material materials with Water content of 0.1 %

ISO 15512

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.05 GPa

Show Supplier Material materials with Elastic modulus of 2.05 GPa

ISO 527-2 (1mm/min)

Elongation

23.0 °C

50 %

Show Supplier Material materials with Elongation of 50 %

min., ISO 527-2 (5mm/min)

Flexural modulus

23.0 °C

1.95 GPa

Show Supplier Material materials with Flexural modulus of 1.95 GPa

ISO 178 (2mm/min)

Flexural strength

23.0 °C

78 MPa

Show Supplier Material materials with Flexural strength of 78 MPa

ISO 178 (2mm/min)

Impact strength, Charpy notched

-30.0 °C

30 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 30 kJ/m²

ISO 179/1eA

23.0 °C

83 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 83 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-40.0 °C

25 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 25 kJ/m²

ISO 180/1A

23.0 °C

80 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 80 kJ/m²

ISO 180/1A

Unlock all property charts

Tensile strength

23.0 °C

45 MPa

Show Supplier Material materials with Tensile strength of 45 MPa

ISO 527-2 (5mm/min)

Impact strength, Charpy unnotched

no break at 23°C; ISO 179/1eU

Impact strength, Izod unnotched

no break at 23°C; ISO 180/1U

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

180 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 180 °C

ISO 75-2/B

Heat deflection temperature, 1.80 MPa

85 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 85 °C

ISO 75-2/A

Melting point

260 °C

Show Supplier Material materials with Melting point of 260 °C

ISO 3146

Flammability

UL94 (0.8mm) HB

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

EN 60112

Surface resistivity

23.0 °C

1.00E+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+14 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1.8 %

Show Supplier Material materials with Shrinkage of 1.8 %

ISO 294-4 (3mm)

Shrinkage, transverse

23.0 °C

2.2 %

Show Supplier Material materials with Shrinkage, transverse of 2.2 %

ISO 294-4 (3mm)

Technological properties

Property
Application areas

Eplamid 66 Impact modified compounds are used in all sectors of industry, offering a good impact strength for mechanical properties and ensures an outstanding performance even at low temperatures (up to -40°C).

Other