EPIMIX PBT FW NC Q101

Want to keep this datasheet? Save it now in your required format

Description

EPIMIX PBT, heat stabilized and lubricated for injection moulding.

EPIMIX PBT is used in all sectors of industry, has and excellent surface finish, low warpage and all around excellent mechanical properties. EPIMIX PBT is approved for applications in direct contact with drinking water and food.

This material data has been provided by Epsan.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.7 GPa

Show Supplier Material materials with Elastic modulus of 2.7 GPa

ISO 527-2 (1mm/min)

Elongation

23.0 °C

8 %

Show Supplier Material materials with Elongation of 8 %

ISO 527-2 (5mm/min)

Flexural modulus

23.0 °C

2.6 GPa

Show Supplier Material materials with Flexural modulus of 2.6 GPa

ISO 178 (2mm/min)

Flexural strength

23.0 °C

85 MPa

Show Supplier Material materials with Flexural strength of 85 MPa

ISO 178 (2mm/min)

Impact strength, Charpy notched

23.0 °C

8 kJ/m²

Show Supplier Material materials with Impact strength, Charpy notched of 8 kJ/m²

ISO 179/1eA

Impact strength, Charpy unnotched

23.0 °C

75 kJ/m²

Show Supplier Material materials with Impact strength, Charpy unnotched of 75 kJ/m²

ISO 179/1eU

Impact strength, Izod notched

23.0 °C

7 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 7 kJ/m²

ISO 180/1A

Impact strength, Izod unnotched

23.0 °C

70 kJ/m²

Show Supplier Material materials with Impact strength, Izod unnotched of 70 kJ/m²

ISO 180/1U

Tensile strength

23.0 °C

65 MPa

Show Supplier Material materials with Tensile strength of 65 MPa

ISO 527-2 (5mm/min)

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

160 °C

Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 160 °C

ISO 75-2/B

Heat deflection temperature, 1.80 MPa

60 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 60 °C

ISO 75-2/A

Melting point

225 °C

Show Supplier Material materials with Melting point of 225 °C

ISO 3146

Flammability

UL94 (0.8mm) HB

Electrical

PropertyTemperatureValueComment

Comparative tracking index

23.0 °C

600 V

Show Supplier Material materials with Comparative tracking index of 600 V

EN 60112

Surface resistivity

23.0 °C

1.00E+13 Ω/sq

Show Supplier Material materials with Surface resistivity of 1.00E+13 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.5 %

Show Supplier Material materials with Shrinkage of 0.5 %

ISO 294-4 (3mm)

Shrinkage, transverse

23.0 °C

1.9 %

Show Supplier Material materials with Shrinkage, transverse of 1.9 %

ISO 294-4 (3mm)

Technological properties

Property
Application areas

EPIMIX PBT is used in all sectors of industry, has and excellent surface finish, low warpage and all around excellent mechanical properties. EPIMIX PBT is approved for applications in direct contact with drinking water and food.

Certifications

Drinking Water,Food Contact

Other