General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.17 g/cm³ Show Supplier Material materials with Density of 1.17 g/cm³ | Calculated |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 0.65 GPa Show Supplier Material materials with Elastic modulus of 0.65 GPa | ASTM D638 |
Flexural modulus | 23.0 °C | 0.62 GPa Show Supplier Material materials with Flexural modulus of 0.62 GPa | ASTM D790 |
Flexural strength | 23.0 °C | 25.3 MPa Show Supplier Material materials with Flexural strength of 25.3 MPa | ASTM D790 |
Tensile strength | 23.0 °C | 16.2 MPa Show Supplier Material materials with Tensile strength of 16.2 MPa | ASTM D638 |
Thermal
Property | Value | Comment |
---|---|---|
Melting point | 130 °C Show Supplier Material materials with Melting point of 130 °C | ASTM D3418 |
Rheological Properties
Property | Value | Comment |
---|---|---|
Melt mass-flow rate | 1.3 g/10min Show Supplier Material materials with Melt mass-flow rate of 1.3 g/10min | ASTM D1238 (190°C/10 kg) |
Technological properties
Property | ||
---|---|---|
Application areas | BioBlend® XD 22620 is designed for blow molding applications that require stress crack resistance, rigidity, and high impact strength. |