NuPlastiQ® BC 27250

Alternative and trade names
NuPlastiQ® BC 27250
Want to keep this datasheet? Save it now in your required format

Description

BioPolymer is a unique type of thermoplastic starch (TPS) resin made from natural, renewable agricultural resources such as potatoes, corn, and cassava and is a 100% USDA Certified Bio-based product.

One of the NuPlastiQ® BC family of biodegradable BioPolymers designed for compostable films and bags. Fully compounded and ready for film production.

Due to NuPlastiQ’s unique properties, it can be homogenously blended with other fossil-based plastics (such as PE, PP & PS) or bio-based materials (such as PLA, PBAT and PHA) to create NuPlastiQ BioBlends that increase the sustainability of all plastic products.

Because of its strength, bags made with 25% NuPlastiQ and 75% PE that are downgauged by 30% result in 50% less fossil fuel feedstocks being used to make the bags. Production of NuPlastiQ also generates 80% less CO2 than traditional resins made from fossil-fuel.

This material data has been provided by Feconix Pte Ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Bio-based content

100 %

Show Supplier Material materials with Bio-based content of 100 %

Density

23.0 °C

1.3 g/cm³

Show Supplier Material materials with Density of 1.3 g/cm³

ASTM D792

Carbon Footprint

0.2

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.24 GPa

Show Supplier Material materials with Elastic modulus of 0.24 GPa

ASTM D638

Elongation

23.0 °C

110 %

Show Supplier Material materials with Elongation of 110 %

ASTM D638

Flexural modulus

23.0 °C

0.31 GPa

Show Supplier Material materials with Flexural modulus of 0.31 GPa

ASTM D790

Tensile strength

23.0 °C

12 MPa

Show Supplier Material materials with Tensile strength of 12 MPa

ASTM D638

Thermal

PropertyValueComment

Melting point

140 - 160 °C

Show Supplier Material materials with Melting point of 140 - 160 °C

ASTM D3418

Rheological Properties

PropertyValueComment

Melt mass-flow rate

2.9 g/10min

Show Supplier Material materials with Melt mass-flow rate of 2.9 g/10min

ASTM D1238 (190°C/2.16 kg)

Technological properties

Property
Application areas

NuPlastiQ® BC 27250 is intended for bags and film applications that require at least 40% bio-content. Used for products that require biodegradation and are intended for compost environments.

Certifications

USDA Certified Bio-based product