ISOTHANE 2095A-MH is a polyester poly(caprolactone)ester based thermoplastic polyurethane. ISOTHANE 2095A-MH exhibits excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stability. ISOTHANE 2095A-MH can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Compression set

100.0 °C

30 [-]

Show Supplier Material materials with Compression set of 30 [-]

ASTM D395, for 22hrs

Elongation

23.0 °C

460 %

Show Supplier Material materials with Elongation of 460 %

ASTM D412

Hardness, Shore A

23.0 °C

95 [-]

Show Supplier Material materials with Hardness, Shore A of 95 [-]

ASTM D2240

Tear strength

23.0 °C

180 kN/m

Show Supplier Material materials with Tear strength of 180 kN/m

ASTM D624

Tensile strength

23.0 °C

33 MPa

Show Supplier Material materials with Tensile strength of 33 MPa