General
Property | Value |
---|---|
Density | 1.45 g/cm³ Show Supplier Material materials with Density of 1.45 g/cm³ |
Mechanical
Property | Temperature | Value |
---|---|---|
Flexural modulus | 11.78 GPa Show Supplier Material materials with Flexural modulus of 11.78 GPa | |
Flexural strength | 305.0 MPa Show Supplier Material materials with Flexural strength of 305.0 MPa | |
Impact strength, Izod notched, ASTM | -20 °C | 294 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 294 J/m |
23 °C | 343 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 343 J/m | |
Tensile strength | 216.0 MPa Show Supplier Material materials with Tensile strength of 216.0 MPa |
Thermal
Property | Value | Pressure | Comment |
---|---|---|---|
Heat deflection temperature | 245.0 °C Show Supplier Material materials with Heat deflection temperature of 245.0 °C | 1.8 MPa | ASTM D648 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Car Industry, Frame in the engine bay, Seat frame, Dashboard frame, Frame of Battery base, Door panel, Pedals, Fender apron, Frame of spare tire. Electronics, High precision plug-in/element, Structure parts of the printer, Frame of the 3C products, Structure parts. Petrochemical, Corrosion and abrasion resistance parts, Grille platform, Parts of filtration facility, Reactor parts. Others, Seat frame of bicycle, Snowboard, Structure parts of the exercise gear and pedals, Toe of Safety boot, Safety helmet. | |
Fillers | 40% Glass Fiber |