PCL 2050D-MH

Alternative and trade names
2050D-MH
Want to keep this datasheet? Save it now in your required format

Description

ISOTHANE 2050D-MH is a polyester poly(caprolactone)ester based thermoplastic polyurethane. ISOTHANE 2050D-MH exhibits excellent toughness, abrasive resistance, solvent resistance, and hydrolysis stability. ISOTHANE 2050D-MH can be injection molded, blow molded, and extruded.

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

1.2 g/cm³

Show Supplier Material materials with Density of 1.2 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Compression set

100 °C

30 [-]

Show Supplier Material materials with Compression set of 30 [-]

ASTM D395, for 22hrs

Elongation

440.0 %

Show Supplier Material materials with Elongation of 440.0 %

ASTM D412

Hardness, Shore D

51.0 [-]

Show Supplier Material materials with Hardness, Shore D of 51.0 [-]

ASTM D2240

Tear strength

180.0 kN/m

Show Supplier Material materials with Tear strength of 180.0 kN/m

ASTM D624

Tensile strength

34.0 MPa

Show Supplier Material materials with Tensile strength of 34.0 MPa

ASTM D638

Technological properties

Property
Application areas

Seals, Gaskets, Sheets, Film, Tube, Cable, Shoe Sole, Sporting Equipment and Mechanical Goods.