Description

Excellent stiffness, Heat resistance, Dimensional stability

This material data has been provided by Great Eastern Resins Industrial Co. ltd.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Density

1.12 g/cm³

Show Supplier Material materials with Density of 1.12 g/cm³

Mechanical

PropertyValueComment

Elongation

2.0 %

Show Supplier Material materials with Elongation of 2.0 %

Flexural modulus

5.886 GPa

Show Supplier Material materials with Flexural modulus of 5.886 GPa

Flexural strength

156.0 MPa

Show Supplier Material materials with Flexural strength of 156.0 MPa

Impact strength, Izod notched, ASTM

156 J/m

Show Supplier Material materials with Impact strength, Izod notched, ASTM of 156 J/m

ASTM D256

Tensile strength

98.0 MPa

Show Supplier Material materials with Tensile strength of 98.0 MPa

Rheological Properties

PropertyValue

Shrinkage

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

0.3 %

Show Supplier Material materials with Shrinkage of 0.3 %

Technological properties

Property
Application areas

Mechanical Parts, Automotive