General
Property | Value |
---|---|
Relative density | 8.82 [-] Show Supplier Material materials with Relative density of 8.82 [-] |
Mechanical
Property | Value | Comment |
---|---|---|
Elastic modulus | 115 GPa Show Supplier Material materials with Elastic modulus of 115 GPa | |
Elongation | 5 % Show Supplier Material materials with Elongation of 5 % | min. | EH Temper | for thickness 0.2-5 mm |
8 % Show Supplier Material materials with Elongation of 8 % | min. | H Temper | for thickness 0.1-5 mm | |
20 % Show Supplier Material materials with Elongation of 20 % | min. | 1/2H Temper | for thickness 0.1-5 mm | |
35 % Show Supplier Material materials with Elongation of 35 % | min. | 1/4H Temper | for thickness 0.1-5 mm | |
42 % Show Supplier Material materials with Elongation of 42 % | min. | O Temper | for thickness 0.1-5 mm | |
Flexural modulus | 105 GPa Show Supplier Material materials with Flexural modulus of 105 GPa | |
Hardness, Vickers | 100 - 160 [-] Show Supplier Material materials with Hardness, Vickers of 100 - 160 [-] | 1/4H Temper | for thickness 0.1-5 mm |
150 - 205 [-] Show Supplier Material materials with Hardness, Vickers of 150 - 205 [-] | 1/2H Temper | for thickness 0.1-5 mm | |
180 - 230 [-] Show Supplier Material materials with Hardness, Vickers of 180 - 230 [-] | H Temper | for thickness 0.1-5 mm | |
200 - 240 [-] Show Supplier Material materials with Hardness, Vickers of 200 - 240 [-] | EH Temper | for thickness 0.05-5 mm | |
210 [-] Show Supplier Material materials with Hardness, Vickers of 210 [-] | min. | SH Temper | for thickness 0.05-5 mm | |
Tensile strength | 315 MPa Show Supplier Material materials with Tensile strength of 315 MPa | min. | O Temper | for thickness 0.1-5 mm |
390 - 510 MPa Show Supplier Material materials with Tensile strength of 390 - 510 MPa | 1/4H Temper | for thickness 0.1-5 mm | |
490 - 610 MPa Show Supplier Material materials with Tensile strength of 490 - 610 MPa | 1/2H Temper | for thickness 0.1-5 mm | |
590 - 685 MPa Show Supplier Material materials with Tensile strength of 590 - 685 MPa | H Temper | for thickness 0.1-5 mm | |
635 - 720 MPa Show Supplier Material materials with Tensile strength of 635 - 720 MPa | EH Temper | for thickness 0.1-5 mm | |
690 MPa Show Supplier Material materials with Tensile strength of 690 MPa | min. | SH Temper | for thickness 0.1-5 mm |
Thermal
Property | Value |
---|---|
Coefficient of thermal expansion | 1.82e-05 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.82e-05 1/K |
Melting point | 900 - 1040 °C Show Supplier Material materials with Melting point of 900 - 1040 °C |
Specific heat capacity | 375 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 375 J/(kg·K) |
Thermal conductivity | 67 W/(m·K) Show Supplier Material materials with Thermal conductivity of 67 W/(m·K) |
Electrical
Property | Value |
---|---|
Specific Electrical conductivity | 14 % IACS Show Supplier Material materials with Specific Electrical conductivity of 14 % IACS |
Chemical properties
Property | Value | Comment |
---|---|---|
Iron | 0.1 % Show Supplier Material materials with Iron of 0.1 % | max. |
Lead | 0.02 % Show Supplier Material materials with Lead of 0.02 % | max. |
Other | 99.5 % Show Supplier Material materials with Other of 99.5 % | min. | Cu+Sn+P |
Phosphorus | 0.03 - 0.35 % Show Supplier Material materials with Phosphorus of 0.03 - 0.35 % | |
Tin | 5.5 - 7 % Show Supplier Material materials with Tin of 5.5 - 7 % | |
Zinc | 0.2 % Show Supplier Material materials with Zinc of 0.2 % | max. |
Technological properties
Property | ||
---|---|---|
Application areas | The grade is particularly suitable for electronics (connectors, lead frames, lead terminals, transistor terminals, etc.), electrical (relay and switch contacts, rotary switch slides and contacts, fuse clips, etc.), automotive (bearing frames, hydraulic equipment caps, packing, bearings, clutch disks, electrical parts, etc.) and others (bellows, slides, blades, plate springs, corrosion-proof machinery equipment, diaphragms, etc.) | |
Coating | Standard product specification of a HOT-DIP-tinned strip. *Width means the slit width after plating. *Different plating thickness for each side is possible. * We can accommodate our products to individual specifications other than the above standard specifications. Please feel free to call us. | |
Other | Hardness Vickers note: Minimum test force is 1.961 N | |
Tolerances |