Properties

General

PropertyTemperatureValue

Density

23.0 °C

18.8 g/cm³

Show Supplier Material materials with Density of 18.8 g/cm³

Dimension

PropertyValue

Dimensions

Dimensions available upon request.

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

180 GPa

Show Supplier Material materials with Elastic modulus of 180 GPa

Elongation

23.0 °C

20 %

Show Supplier Material materials with Elongation of 20 %

min.

Hardness, Vickers

23.0 °C

220 - 230 [-]

Show Supplier Material materials with Hardness, Vickers of 220 - 230 [-]

Shear modulus

23.0 °C

74 GPa

Show Supplier Material materials with Shear modulus of 74 GPa

Tensile strength

23.0 °C

620 - 710 MPa

Show Supplier Material materials with Tensile strength of 620 - 710 MPa

Yield strength Rp0.2

23.0 °C

410 - 460 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 410 - 460 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.02E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.02E-5 1/K

RT-100 °C

Melting point

1660 - 1700 °C

Show Supplier Material materials with Melting point of 1660 - 1700 °C

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

2.98E-7 - 3.04E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 2.98E-7 - 3.04E-7 Ω·m

Specific Electrical conductivity

5.6 - 5.77 % IACS

Show Supplier Material materials with Specific Electrical conductivity of 5.6 - 5.77 % IACS

Temperature coefficient of resistance

23.0 °C

1.25E-3 - 1.35E-3 1/K

Show Supplier Material materials with Temperature coefficient of resistance of 1.25E-3 - 1.35E-3 1/K

0-100 °C

Technological properties

Property
Application areas

Spark plugs, electrodes

Corrosion properties

Corrosion resistant

Other

Ductile