See where Platinum (Pt) falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.
Density
ρ21.45 g/cm³ at 23 °C
Melting point
Tm1769 °C
Thermal conductivity
λ69.11 W/(m·K) at 20 °C
Electrical resistivity
ρel9.83E-8 Ω·m at 20 °C
This material data has been provided by Heraeus.