Pt10Rh

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Heraeus.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

20 g/cm³

Show Supplier Material materials with Density of 20 g/cm³

Mechanical

PropertyTemperatureValueComment

Creep strength

1200.0 °C

2.4 MPa

Show Supplier Material materials with Creep strength of 2.4 MPa

10,000 h (extrapolated data)

1400.0 °C

1.3 MPa

Show Supplier Material materials with Creep strength of 1.3 MPa

10,000 h (extrapolated data)

1600.0 °C

0.5 MPa

Show Supplier Material materials with Creep strength of 0.5 MPa

10,000 h (extrapolated data)

Elastic modulus

23.0 °C

213 GPa

Show Supplier Material materials with Elastic modulus of 213 GPa

Elongation

20.0 °C

38 %

Show Supplier Material materials with Elongation of 38 %

1200.0 °C

42 %

Show Supplier Material materials with Elongation of 42 %

1400.0 °C

30 %

Show Supplier Material materials with Elongation of 30 %

1600.0 °C

54 %

Show Supplier Material materials with Elongation of 54 %

Unlock all property charts

Hardness, Vickers

23.0 °C

94 [-]

Show Supplier Material materials with Hardness, Vickers of 94 [-]

Norton Exponent

1200.0 °C

3.6 [-]

Show Supplier Material materials with Norton Exponent of 3.6 [-]

1400.0 °C

3.6 [-]

Show Supplier Material materials with Norton Exponent of 3.6 [-]

1600.0 °C

3.8 [-]

Show Supplier Material materials with Norton Exponent of 3.8 [-]

Unlock all property charts

Tensile strength

20.0 °C

301 MPa

Show Supplier Material materials with Tensile strength of 301 MPa

1200.0 °C

58.8 MPa

Show Supplier Material materials with Tensile strength of 58.8 MPa

1400.0 °C

35.4 MPa

Show Supplier Material materials with Tensile strength of 35.4 MPa

1600.0 °C

16.7 MPa

Show Supplier Material materials with Tensile strength of 16.7 MPa

Unlock all property charts

Yield strength Rp0.2

20.0 °C

134 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 134 MPa

1200.0 °C

44.3 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 44.3 MPa

1400.0 °C

27.7 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 27.7 MPa

1600.0 °C

14.7 MPa

Show Supplier Material materials with Yield strength Rp0.2 of 14.7 MPa

Unlock all property charts

Thermal

PropertyTemperatureValue

Melting point

1840 - 1870 °C

Show Supplier Material materials with Melting point of 1840 - 1870 °C

Thermal conductivity

20.0 °C

40.1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 40.1 W/(m·K)

1200.0 °C

70.6 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 70.6 W/(m·K)

1400.0 °C

70.8 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 70.8 W/(m·K)

Unlock all property charts

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

2.1E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 2.1E-7 Ω·m

1153.0 °C

5.3E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.3E-7 Ω·m

1400.0 °C

5.9E-7 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.9E-7 Ω·m