High Purity Aluminium 99.99% (4N)

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Hydro Aluminium High Purity GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

Property

Aluminium

Balance

Iron

3.0000000000000003E-4 %

Magnesium

1E-4 %

Silicon

3.0000000000000003E-4 %