This material data has been provided by Hydro Aluminium High Purity GmbH.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

Property

Aluminium

Balance

Antimony

1E-6 %

Arsenic

1E-6 %

Barium

2E-6 %

Beryllium

1E-6 %

Bismuth

1E-6 %

Boron

2E-6 %

Caesium

1E-6 %

Calcium

2E-6 %

Cerium

1E-6 %

Chlorine

1E-6 %

Chromium

3E-6 %

Cobalt

1E-6 %

Copper

8E-6 %

Fluorine

1E-6 %

Gallium

1E-6 %

Germanium

1E-6 %

Indium

1E-6 %

Iron

7E-6 %

Lanthanum

1E-6 %

Lead

1E-6 %

Lithium

1E-6 %

Magnesium

8E-6 %

Manganese

2E-6 %

Molybdenum

1E-6 %

Nickel

1E-6 %

Phosphorus

1E-5 %

Platinum

5E-6 %

Silicon

1E-5 %

Silver

1E-6 %

Sodium

1E-6 %

Sulfur

5E-6 %

Thorium

1E-8 %

Tin

1E-6 %

Titanium

4E-6 %

Tungsten

1E-6 %

Uranium

1E-8 %

Vanadium

4E-6 %

Zinc

1E-6 %

Zirconium

1E-6 %