Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
High Purity Aluminium 4N8A
This material data has been provided by Hydro Aluminium High Purity GmbH.
All categories
Chemical properties
Property | ||
---|---|---|
Aluminium | Balance | |
Barium | 1E-5 % | |
Boron | 1E-5 % | |
Calcium | 2E-5 % | |
Chromium | 1E-5 % | |
Gallium | 1E-5 % | |
Iron | 2E-5 % | |
Lead | 1E-5 % | |
Magnesium | 2E-5 % | |
Manganese | 1E-5 % | |
Nickel | 1E-5 % | |
Phosphorus | 5E-5 % | |
Silicon | 3E-5 % | |
Silver | 1E-5 % | |
Sodium | 5E-5 % | |
Titanium | 1E-5 % | |
Vanadium | 2E-5 % | |
Zinc | 1E-5 % | |
Zirconium | 2E-5 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2021 Matmatch GmbH, All rights reserved.
Made with ♥ in Munich!