Chemical properties
Property | ||
---|---|---|
Aluminium | Balance | |
Antimony | 8E-6 % | |
Arsenic | 5E-6 % | |
Barium | 2E-6 % | |
Beryllium | 1E-6 % | |
Bismuth | 5E-6 % | |
Boron | 2E-6 % | |
Caesium | 5E-6 % | |
Calcium | 7E-6 % | |
Cerium | 1.5E-5 % | |
Chlorine | 1E-5 % | |
Chromium | 4E-6 % | |
Cobalt | 1E-6 % | |
Copper | 3E-5 % | |
Fluorine | 1E-5 % | |
Gallium | 1E-6 % | |
Germanium | 1E-5 % | |
Indium | 5E-6 % | |
Iron | 3E-5 % | |
Lanthanum | 7E-6 % | |
Lead | 5E-6 % | |
Lithium | 1E-6 % | |
Magnesium | 3E-5 % | |
Manganese | 2E-6 % | |
Molybdenum | 2E-6 % | |
Nickel | 5E-6 % | |
Phosphorus | 5E-5 % | |
Platinum | 1E-5 % | |
Silicon | 3E-5 % | |
Silver | 5E-6 % | |
Sodium | 5E-6 % | |
Sulfur | 1E-5 % | |
Tin | 5E-6 % | |
Titanium | 5E-6 % | |
Tungsten | 5E-6 % | |
Vanadium | 1E-5 % | |
Zinc | 5E-6 % | |
Zirconium | 3E-6 % |